The use of cold laminating machine skills
Glazing machine manufacturers tell you the laminating machine cold mounting process is what
1. Be sure to wait for the blot to dry before laminating, otherwise it will cause blistering or hair pulling phenomenon.
2, the temperature is generally controlled to 40 ~ 60℃. Too high temperature will make paper and film deformation, resulting in product curling, but not too low, otherwise it will cause insufficient viscosity. The temperature of coated paper should be slightly lower than uncoated paper.
3. The product to be constructed must be flat. There are "flounces" and "tight edge" phenomenon of uneven paper to be processed. "Flounces" paper can be baked, "tight edge" paper can be hung.
4. The laminating machine should also pay attention to the direction of the paper thread, especially the thick paper, to reduce the phenomenon of paper crimping due to rolling and stretching.
5. When printing, spray powder as little as possible, otherwise it will cause empty foaming at the pile of powder. Before the film should be dusted off, printing can be hung to dry powder, printing can be less manual wiping.